Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 9.93 MPa | 1440 psi | ASTM D882 |
Dow AFFINITY™ PL 1850G Polyolefin Plastomer (POP) AFFINITY™ PL 1840G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed to provide blown and cast film products with low temperature sealability, excellent optics and g.. |
|||
Film Tensile Strength at Yield, MD | 9.90 MPa | 1440 psi | |