Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 9.70 MPa | 1410 psi | ASTM D882 |
ExxonMobil Escorene® LD-104 LDPE Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer packaging film resin with excellent clarity and good stiffness. It is excellent either blown film or chill roll casting equipment. I.. |
|||
Film Tensile Strength at Yield, MD | 9.70 MPa | 1410 psi | ASTM D882 |
ExxonMobil Escorene® LD-113 LDPE General Purpose Packaging Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin that offers a good balance of toughness, drawdown capability, stiffness and clarity. LD-113 exhibits good machinability in.. |
|||
Film Tensile Strength at Yield, MD | 9.70 MPa | 1410 psi | ASTM D882 |
ExxonMobil Escorene® LD-134 LDPE Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity. It is suitable for processing in blown film equipment and can be drawn down to 1.0 mil.Applications: Fo.. |
|||
Film Tensile Strength at Yield, MD | 9.70 MPa | 1410 psi | ASTM D882 |
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su.. |