Polymer Property : Film Tensile Strength at Yield, MD = 32.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 32.0 MPa
4640 psi
ISO 527
Premix Thermoplastics PRE-ELEC® PET 1451
PRE-ELEC PET 1451 is a conductive thermoplastic compound based on PETG. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PET 14..
Film Tensile Strength at Yield, MD 32.0 MPa
4640 psi
ISO 1184
SIDPEC EGYPTENE® HD 5301 FB HDPE Film
Applications:Strong thin filmCarrier bagGrocery sacksFilm properties were measured on 15 micron film extruded at a blow up ratio of 5:1, 8D neck height.Information provided by Interchim s.r.l., offi..
Film Tensile Strength at Yield, MD 32.0 MPa
4640 psi
parallel; ISO 527-3
DSM Akulon® F127 PA6
Low/Medium Viscosity, Film Extrusion
Film Tensile Strength at Yield, MD 32.0 MPa
4640 psi
parallel; ISO 527-3
DSM Akulon® F132 PA6
Film Extrusion, High Viscosity
Film Tensile Strength at Yield, MD 32.0 MPa
4640 psi
parallel; ISO 527-3
DSM Akulon® F132-C1 PA6
Film Extrusion, High Viscosity, Lubricated
Film Tensile Strength at Yield, MD 32.0 MPa
4640 psi
parallel; ISO 527-3
DSM Akulon® F234-C PA6
Film Extrusion, High Viscosity, Lubricated
Film Tensile Strength at Yield, MD 32.0 MPa
4640 psi
parallel; ISO 527-3
DSM Akulon® F128 PA6
Film Extrusion, Medium Viscosity
Film Tensile Strength at Yield, MD 32.0 MPa
4640 psi
ASTM D882
ExxonMobil Escorene® HDZ-128 MMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.Can be processed on high stalk, pocket extrusion or cast lines. Films made from HDZ-128 exhibit an excellent stiffness balance. High thermal stabi..