Polymer Property : Film Tensile Strength at Yield, MD = 26.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 26.9 MPa
3900 psi
ASTM D882
ExxonMobil Escorene™ LD 706.15 Cast Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 706.15 is a 14.9 wt% vinyl acetate copolymer film resin designed for coextruded cast film applications.Availability: Latin America, North America and South Ame..