Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 24.1 MPa | 3500 psi | ASTM D822 |
LyondellBasell Alathon® M6060 High Density Polyethylene ApplicationsALATHON M 6060 is a medium molecular weight high density homopolymer with extremely low gel content. This resin provides high stiffness and narrow molecular weight distribution for use .. |
|||
Film Tensile Strength at Yield, MD | 24.1 MPa | 3500 psi | 10 in/min; ASTM D-882 |
Bapolene® 105F Low Density Polyethylene Film Resin Description: Bapolene LD105F is an unmodified low density polyethylene which extrudes into a low gloss high impact film. It contains antiblock additives and no slip additives. This product meets th.. |
|||
Film Tensile Strength at Yield, MD | 24.1 MPa | 3500 psi | ASTM D 882 A |
Total Finathene® HL 328 HDPE resin
(discontinued **) Applications: Specialty merchandise bags, millinery/notion bags, mailing envelopes, heavy-duty shipping sacks, shrink films, fresh cut produce packaging, coextrusionInformation provided provided by .. |