Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 15.9 MPa | 2300 psi | ASTM D882 |
Dow DAF 780 Carpet Underlayment Adhesion Film DAF 780 is a low melt point, coextruded film used to improve slip characteristics of polyurethane foam for carpet installation or other applications.Information provided by Dow |
|||
Film Tensile Strength at Yield, MD | 15.9 MPa | 2310 psi | ASTM D882 |
Bapolene® 122F Polyethylene, Film Grade Bapolene LL122F is a general purpose LLDPE for blown film extrusion applications. This resin offers excellent tensile and toughness properties. Contains medium levels of slip/antiblock additives. .. |
|||
Film Tensile Strength at Yield, MD | 15.9 MPa | 2300 psi | ASTM D882 |
ExxonMobil Enable™ 35-05CH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 35-05CH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |