Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.3 MPa
1640 psi
ASTM D882
ExxonMobil Exceed™ 377D60 LDPE/Hexene Tough Premium Film Resin, 3 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 377D60 resin exhibit excellent impact strength and b..
Film Tensile Strength at Yield, MD 11.3 MPa
1640 psi
Dow Elite® 5400 Linear Low Density Polyethylene
5400 enhanced polyethylene resin is a copolymer produced via INSITE technology from Dow Plastics. It offers extremely high impact resistance, combined with excellent tear, tensile, and optical prop..