Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 10.1 MPa | 1460 psi | ASTM D882 |
ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 0.6 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE film resin. Films made from LL-3001 have outstanding tensile and toughness properties. The superior strength properties a.. |
|||
Film Tensile Strength at Yield, MD | 10.1 MPa | 1460 psi | at 2% offset; ASTM D882 |
ExxonMobil LD 135.09 Blown Film Resin
(discontinued **) LD 135.09 is a homopolymer film resin with good clarity. Applications include food packaging, light to medium duty bags, and textile packaging.Information provided by ExxonMobil Chemical |