Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.210 MPa-m/sec | 6000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Ertalyte® TX Internally Lubricated Semi-Crystalline Polyester (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.210 MPa-m/sec | 6000 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP Ketron® 1000 PEEK unfilled, extruded (ISO Data) Ketron PEEK-1000 stock shapes are produced from virgin polyetheretherketone resin and offer the highest toughness and impact strength of all Ketron PEEK grades. Both Ketron PEEK-1000 natural & black.. |
|||
Limiting Pressure Velocity | 0.210 MPa-m/sec | 6000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Nylatron® LFG (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.210 MPa-m/sec | 6000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Nylatron® LIG Oil Filled Cast 6 Nylon (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.210 MPa-m/sec | 6000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Semitron® MPR-1000 (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.210 MPa-m/sec | 6000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP TIVAR® HPV UHMW-PE (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.210 - 1.26 MPa-m/sec | 6000 - 36000 psi-ft/min | Average value: 0.509 MPa-m/sec Grade Count:11 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
Limiting Pressure Velocity | 0.210 MPa-m/sec | 6000 psi-ft/min | 4:1 safety factor applied; QTM 55010 |
Quadrant EPP Semitron® CMP LL5 Polyester (ASTM Product Data Sheet) Enhanced semi-crystalline polyester product for extended service in CMP retaining rings. Superior performance, especially in oxide processes, and cost effective relative to standard ring materials. .. |
|||
Limiting Pressure Velocity | 0.210 MPa-m/sec | 6000 psi-ft/min | LNP EPALP-TB003, at 100 ft/min |
Ensinger HYDEX® 4101 Polybutylene Terephthalate (PBT) HYDEX® 4101 & 4101L (lubricated) is a very stable chemical compound that can withstand high impact without deterioration. It is approved for direct contact with food by the FDA and is ideal for ma.. |
|||
Limiting Pressure Velocity | 0.210 MPa-m/sec | 6000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Semitron® ESd 500 HR PTFE, static dissipative, compression molded (ASTM Product Data Sheet) |