Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 1.75 MPa-m/sec | 50000 psi-ft/min | |
Trelleborg Sealing Solutions HiMod® 913 Thermoplastic Bearing Thermoplastic BearingCharacteristics: HiMod® 913 is a self lubrication bearing material made for precise applications requiring continuous use at temperatures up to 400°F, or high PV performance. .. |
|||
Limiting Pressure Velocity | 1.75 MPa-m/sec | 50000 psi-ft/min | Unlubricated. Max P = 36,000 psi and max V = 1000 fpm |
TriStar TriSteel PR Metal Backed PTFE Bearing System Ultraflon 602e enhanced PTFE (PR) lined metal backed bearing , high speed reciprocating, self lubricating, high temperature and high load applications. Liner is designed specifically for high freque.. |
|||
Limiting Pressure Velocity | 1.75 MPa-m/sec | 50000 psi-ft/min | Unlubricated. Max P = 36,000 psi and max V = 1000 fpm |
TriStar TriSteel PT Metal Backed PTFE Bearing System Ultraflon 602 (PT) PTFE lined metal backed bearing system, low friction, high PV, high speed sleeve, flange and thrust bearings, zero lube required, high operating temperature. Ultraflon 602 PTFE Li.. |