Polymer Property : Limiting Pressure Velocity = 170000 psi-ft/min Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 5.96 MPa-m/sec
170000 psi-ft/min
1200 in/min
Ensinger Tecapeek® Polyetheretherketone (PEEK)
Tecapeek™, made from Victrex PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance.Excellent flex..
Copyright © lookpolymers.com All Rights Reserved