Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.0500 MPa-m/sec | 1430 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP Borotron® HM PE-HMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
Limiting Pressure Velocity | 0.0500 MPa-m/sec | 1430 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP Borotron® UH PE-UHMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
Limiting Pressure Velocity | 0.0500 MPa-m/sec | 1430 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP PE 500 PE-HMW, virgin (ISO Data) This grade exhibits a good combination of stiffness, toughness, mechanical damping ability with wear- and abrasion resistance and can easily be welded. In less demanding applications with respect to.. |
|||
Limiting Pressure Velocity | 0.0500 MPa-m/sec | 1430 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP TIVAR® 1000 antistatic PE-UHMW + carbon black (ISO Data) By incorporating an effective carbon black grade, TIVAR 1000 antistatic offers the electrostatic dissipative properties often required for PE-UHMW components operating at high line speeds and convey.. |
|||
Limiting Pressure Velocity | 0.0500 MPa-m/sec | 1430 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP TIVAR® 1000 ASTL PE-UHMW + specific additives (ISO Data) TIVAR 1000 ASTL, based on a PE-UHMW grade with extremely high molecular weight, has been specifically developed for tough anti-abrasion applications. TIVAR 1000 ASTL shows a higher wear and abrasion.. |
|||
Limiting Pressure Velocity | 0.0500 MPa-m/sec | 1430 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP TIVAR® 1000 EC PE-UHMW + specific additives (ISO Data) TIVAR 1000 EC is a PE-UHMW grade containing specific additives rendering this material a lower surface resistivity than TIVAR 1000 antistatic, improving electrical conductivity and UV-resistance |
|||
Limiting Pressure Velocity | 0.0500 MPa-m/sec | 1430 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP TIVAR® 1000 PE-UHMW, virgin (ISO Data) TIVAR 1000 exhibits a very well balanced property profile. It combines a very good wear and abrasion resistance with an outstanding impact strength, even at temperatures below -200°C. |
|||
Limiting Pressure Velocity | 0.0500 MPa-m/sec | 1430 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP TIVAR® Burnguard PE-UHMW + flame retardant + other additives (ISO Data) TIVAR Burnguard is a PE-UHMW grade containing a very effective non-halogenated flame retardant. Specifically developed to improve the poor flammability behaviour of straight forward virgin polyethyl.. |
|||
Limiting Pressure Velocity | 0.0500 MPa-m/sec | 1430 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP TIVAR® Ceram P PE-UHMW + micro glass beads + other additives (ISO Data) TIVAR Ceram P is a wear improved PE-UHMW material with incorporated micro glass beads, specifically developed for use in the dewatering zone of paper machinery equipped with plastic wires and manufa.. |
|||
Limiting Pressure Velocity | 0.0500 MPa-m/sec | 1430 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP TIVAR® Cleanstat PE-UHMW + specific additives (ISO Data) TIVAR CleanStat is a PE-UHMW grade for use in food processing and pharmaceutical industries. It exhibits static dissipative properties and has a food contact compliant composition. Very good wear an.. |
|||
Limiting Pressure Velocity | 0.0500 MPa-m/sec | 1430 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP TIVAR® Dryslide PE-UHMW + internal lubricant + other additives (ISO Data) Thanks to the lubricant built into a PE-UHMW matrix with higher molecular weight, TIVAR DrySlide offers a lower coefficient of friction and enhanced wear and abrasion resistance than TIVAR 1000. The.. |
|||
Limiting Pressure Velocity | 0.0500 MPa-m/sec | 1430 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP TIVAR® DS PE-UHMW + additives (ISO Data) TIVAR DS is a modified PE-UHMW with extremely high molecular weight. The latter in combination with a particular manufacturing process result in a PE-UHMW grade with superior wear and abrasion resis.. |
|||
Limiting Pressure Velocity | 0.0500 MPa-m/sec | 1430 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP TIVAR® ECO PE-UHMW reprocessed (ISO Data) This grade, partially composed of reprocessed PE-UHMW material, has an overall lower property level than the virgin TIVAR 1000 and a lower cost. Compared with virgin PE 500, however, it has a much b.. |
|||
Limiting Pressure Velocity | 0.0500 MPa-m/sec | 1430 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP TIVAR® H.O.T. PE-UHMW + specific additives (ISO Data) TIVAR H.O.T. [Higher Operating Temperature] is formulated to maintain inherent PE-UHMW key properties over an extended service temperature range, in this way considerably increasing part life in low.. |
|||
Limiting Pressure Velocity | 0.0500 MPa-m/sec | 1430 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP TIVAR® MD PE-UHMW + metal detectable additive (ISO Data) This PE-UHMW grade with extremely high degree of polymerisation contains a metal detectable additive which does hardly affect the inherent PE-UHMW key properties. TIVAR MD presents excellent toughne.. |
|||
Limiting Pressure Velocity | 0.0500 MPa-m/sec | 1430 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP TIVAR® Oil Filled PE-UHMW + oil (ISO Data) TIVAR Oil Filled is a self-lubricating PE-UHMW material in the real meaning of the word. Next to an enhanced wear resistance, the incorporated and evenly dispersed oil renders this material a consid.. |
|||
Limiting Pressure Velocity | 0.0500 MPa-m/sec | 1430 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP TIVAR® SuperPlus PE-UHMW + specific additives (ISO Data) TIVAR SuperPlus is a wear optimised, partially cross-linked PE-UHMW material with extremely high degree of polymerisation for use in most demanding applications and environments. When used for drain.. |
|||
Limiting Pressure Velocity | 0.0500 MPa-m/sec | 1430 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP TIVAR® TECH PE-UHMW + MoS2 (ISO Data) This PE-UHMW grade with extremely high degree of polymerisation contains molybdenum disulphide, resulting in a material with improved wear resistance and sliding properties over TIVAR 1000. |
|||
Limiting Pressure Velocity | 0.0500 - 0.210 MPa-m/sec | 1430 - 6000 psi-ft/min | Average value: 0.0852 MPa-m/sec Grade Count:38 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |