Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.740 MPa-m/sec | 21100 psi-ft/min | |
Kuraray Genestarâ„¢ N1006D-H31 Nylon Standard unreinforced extrusion grade. Main Features:Chemical resistanceLong term heat resistanceExample of applications:Tube applications |