Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.320 MPa-m/sec | 9140 psi-ft/min | at 0.1 m/s unlubricated |
Quadrant EPP Duratron® PAI T4203 PAI, unfilled, extruded (ISO Data) Duratron T4203 PAI offers the best toughness and impact strength of all Duratron PAI grades. This extruded Duratron PAI grade is very popular for precision parts in high-tech equipment. In addition,.. |
|||
Limiting Pressure Velocity | 0.320 MPa-m/sec | 9140 psi-ft/min | at 0.1 m/s unlubricated |
Quadrant EPP Duratron® PAI T4503 PAI, unfilled, compression moulded (ISO Data) Compression moulded Duratron T4503 PAI is similar in composition to Duratron T4203 PAI, and is selected when larger shapes are required Very high maximum allowable service temperature in air (250°C.. |
|||
Limiting Pressure Velocity | 0.320 MPa-m/sec | 9140 psi-ft/min | |
Trelleborg Sealing Solutions HiMod® 912 Thermoplastic Bearing Thermoplastic BearingCharacteristics: HiMod® 912 was developed for application with intermittent temperature of 200°F, but requiring a more demanding bearing material with higher performance, imp.. |