Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.298 MPa-m/sec | 8500 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Ketron® 1000 IM Injection Molded Unfilled Polyetheretherketone (ASTM Product Data Sheet) Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to hot water or steam |
|||
Limiting Pressure Velocity | 0.298 MPa-m/sec | 8500 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Ketron® 1000 LSG PEEK, Biocompatibility tested (ISO Product Data Sheet) KETRON® PEEK LSG natural / black stock shapes are produced from batches of Victrex PEEK. This material exhibits a unique combination of mechanical properties, temperature and chemical resistance. .. |
|||
Limiting Pressure Velocity | 0.298 MPa-m/sec | 8500 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Ketron® 1000 LSG PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Datasheet) |
|||
Limiting Pressure Velocity | 0.298 MPa-m/sec | 8500 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Ketron® 1000 PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.298 MPa-m/sec | 8500 psi-ft/min | 4:1 safety factor |
Technetics Group Amicon™ PEEK
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Limiting Pressure Velocity | 0.298 MPa-m/sec | 8500 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Ketron® LSG PEEK-CLASSIX Biocompatibility tested (ASTM Product Data Sheet) KETRON® PEEK-CLASSIX LSG white stock shapes are produced from Invibio® PEEK-CLASSIX White resin. This material exhibits a unique combination of mechanical properties, temperature and chemical re.. |