Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.250 MPa-m/sec | 7140 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP Fluorosint® 207 PTFE + mica, compression moulded (ISO Data) This material has a food contact compliant composition which, in combination with the good mechanical performance, dimensional stability, sliding and wear properties and inherent outstanding chemica.. |
|||
Limiting Pressure Velocity | 0.250 MPa-m/sec | 7140 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data) Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties Hig.. |
|||
Limiting Pressure Velocity | 0.250 MPa-m/sec | 7140 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP Fluorosint® HPV PTFE + additives, bearing grade, compression moulded (ISO Data) FDA compliant Fluorosint HPV is a high performance Fluorosint bearing grade, optimized for high pressure-velocity capabilities and very low wear. Fluorosint HPV was developed for bearing application.. |
|||
Limiting Pressure Velocity | 0.250 MPa-m/sec | 7140 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP Nylatron® NSM PA 6 + internal lubricant, cast (ISO Data) Nylatron NSM is a proprietary cast nylon 6 formulation containing solid lubricant additives which grant this materials self-lubricity, excellent frictional behaviour, superior wear resistance and ou.. |
|||
Limiting Pressure Velocity | 0.250 - 0.400 MPa-m/sec | 7140 - 11400 psi-ft/min | Average value: 0.310 MPa-m/sec Grade Count:4 |
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi.. |
|||
Limiting Pressure Velocity | 0.250 MPa-m/sec | 7140 psi-ft/min | v = 1m/min |
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor.. |