Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.100 MPa-m/sec @Pressure 1.75 MPa |
2860 psi-ft/min @Pressure 254 psi |
31.4 m/min |
Nylacast POM C Acetal Copolymer The copolymer grade is the ideal combination of strength, stiffness and wears resistance. It absorbs very little moisture, is easily machinable and is genuinely porosity-free making it the preferred.. |
|||
Limiting Pressure Velocity | 0.100 MPa-m/sec | 2860 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP Ertacetal® C POM-C, extruded (ISO Data) Ertacetal C is Quadrant’s copolymer acetal grade. Next to the standard natural and black grades, there is also a series of special colours available all showing an FDA food contact compliant compos.. |
|||
Limiting Pressure Velocity | 0.100 MPa-m/sec | 2860 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP Ertacetal® H POM-H, extruded (ISO Data) Ertacetal H is Quadrant’s homopolymer acetal grade. It offers a higher mechanical strength, stiffness, hardness and creep resistance as well as a lower thermal expansion rate and often also a bette.. |
|||
Limiting Pressure Velocity | 0.100 MPa-m/sec | 2860 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP Ertalon® 4.6 PA 4.6, extruded (ISO Data) Compared with conventional nylons, Ertalon 4.6 features a better retention of stiffness and creep resistance over a wide range of temperatures as well as superior heat ageing resistance. Therefore, .. |
|||
Limiting Pressure Velocity | 0.100 MPa-m/sec | 2860 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP Symalit® 1000 PVDF unfilled, extruded (ISO Data) Symalit 1000 PVDF is a highly crystalline unreinforced fluoropolymer combining good mechanical, thermal and electrical properties with excellent chemical resistance. It also shows good resistance to.. |
|||
Limiting Pressure Velocity | 0.100 MPa-m/sec | 2860 psi-ft/min | |
Global EPP PA 66E Extruded Polyamide 66 Polyamides, commonly referred to as nylons, are macromolecular, partially crystalline thermoplastics. Their physical properties are mainly determined by the composition and structure of their molecu.. |
|||
Limiting Pressure Velocity | 0.100 MPa-m/sec | 2860 psi-ft/min | |
Global EPP POM C Acetal Copolymer Polyacetals are highly crystalline thermoplastics, characterised by their high mechanical strength, rigidity and impact resistance. Acetal absorbs very little moisture, enabling the product to maint.. |
|||
Limiting Pressure Velocity | 0.100 MPa-m/sec | 2860 psi-ft/min | v = 200m/min |
Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy Main Characteristics: Modified friction wear; Tough; Soft; Reduced wear at temperatures at 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInfor.. |