Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.0560 MPa-m/sec
1600 psi-ft/min
100 fpm
Ensinger Tecaform™ HPV 13 Acetal Homopolymer - Extruded Products (POM)
Tecaform™ HPV 13 is a brown homopolymer acetal with an internal PTFE lubricant. Its low coefficient of friction, excellent PV values, toughness, wear resistance, and machinability make it an excep..
Limiting Pressure Velocity 0.0560 - 9000 MPa-m/sec
1600 - 2.57e+8 psi-ft/min
Average value: 1500 MPa-m/sec Grade Count:4
Overview of materials for Acetal Homopolymer, PTFE-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o..