Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 680 MPa @Treatment Temp. 593 °C, Time 3.60e+6 sec |
98600 psi @Treatment Temp. 1100 °F, Time 1000 hour |
0.2%. Room temp test after thermal exposure |
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Tensile Strength, Yield | 680 MPa @Strain 0.200 %, Temperature 20.0 °C |
98600 psi @Strain 0.200 %, Temperature 68.0 °F |
Longitudinal |
Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy INCONEL® alloy MA 758 is an oxide-dispersion-strengthened (ODS) nickel-chromium superalloy, made by mechanical alloying. It is a development of the well-established aerospace superalloy, INCONEL.. |
|||
Tensile Strength, Yield | 680 MPa @Strain 0.200 % |
98600 psi @Strain 0.200 % |
as cast |
Wieland Auropal 1 Casting Alloy Gold-silver casting alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, acrylic veneeringDental |
|||
Tensile Strength, Yield | 680 MPa @Strain 0.200 % |
98600 psi @Strain 0.200 % |
hardened |
Wieland Auropal 1 Casting Alloy Gold-silver casting alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, acrylic veneeringDental |
|||
Tensile Strength, Yield | 680 MPa @Strain 0.200 % |
98600 psi @Strain 0.200 % |
30% Cold Worked |
AK Steel 439 ULTRA FORM® Stainless Steel AK Steel 439 ULTRA FORM™ was developed for applications requiring oxidation and corrosion resistance superior to Type 409 as well as superior formability to AK Steel 439 Stainless Steel. As a resul.. |