Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 6.32 MPa @Strain 100 % |
916 psi @Strain 100 % |
ASTM D1708 |
DSM Biomedical PurSil® 35 Thermoplastic Silicone Polyether Polyurethane (TSPU) A novel copolymer that is strong yet flexible with proven biocompatibility and biostability