Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 625 MPa @Strain 0.200 %, Temperature 700 °C |
90600 psi @Strain 0.200 %, Temperature 1290 °F |
|
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Age-hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |