Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 597 MPa @Temperature 649 °C, Time 45700 sec |
86600 psi @Temperature 1200 °F, Time 12.7 hour |
As Welded, Solution Annealed, and Aged; Base/Base Fracture; 0.2% Offset |
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |