Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 541 MPa @Temperature 177 °C |
78500 psi @Temperature 351 °F |
|
Hexcel® HexPly® F263 Epoxy Resin, W3T282 Carbon Fabric Hexcel designation: W3T282-42"-F263; Fiber: T300 CelionInformation provided by HexCel |
|||
Tensile Strength, Yield | 541 MPa @Strain 0.200 % |
78500 psi @Strain 0.200 % |
15% Cold Worked |
AK Steel 409 ULTRA FORM® Stainless Steel AK Steel 409 ULTRA FORM Stainless Steel provides an outstanding combination of improved forming and welding characteristics, while providing superior resistance to oxidation, corrosion, ridging and .. |