Polymer Property : Tensile Strength, Yield = 769 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 5.30 MPa

@Strain 10.0 %
769 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® PL420-H Injection Molding Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 5.30 MPa

@Strain 10.0 %
769 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® PL420-H Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 5.30 MPa

@Strain 5.00 %
769 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® PL461 Injection Molding Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 5.30 MPa

@Strain 5.00 %
769 psi

@Strain 5.00 %
ISO 527-1/-2
DSM Arnitel® PL461 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..