Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 486 MPa @Strain 0.200 % |
70500 psi @Strain 0.200 % |
10% Cold Worked |
AK Steel 409 ULTRA FORM® Stainless Steel AK Steel 409 ULTRA FORM Stainless Steel provides an outstanding combination of improved forming and welding characteristics, while providing superior resistance to oxidation, corrosion, ridging and .. |
|||
Tensile Strength, Yield | 486 MPa @Diameter 12.7 mm, Temperature 25.0 °C |
70500 psi @Diameter 0.500 in, Temperature 77.0 °F |
0.2% Offset |