Polymer Property : Tensile Strength, Yield = 704 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.85 MPa

@Strain 50.0 %
704 psi

@Strain 50.0 %
ASTM D1708
DSM Biomedical CarboSil® 20 80A Thermoplastic Silicone Polycarbonate Polyurethane (TSPCU)
A ground-breaking copolymer that combines the biocompatibility and biostability of conventional silicone elastomers with the processability and toughness of thermoplastic polycarbonate-urethanes Th..