Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 48.3 MPa @Temperature 23.9 °C |
7000 psi @Temperature 75.0 °F |
0° Direction, Dry; CMC form; ASTM D638 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, C2 Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
Tensile Strength, Yield | 48.3 MPa @Thickness 1.57 mm |
7000 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP315 Cotton Fabric Description: Canvas phenolic laminate with graphite added as a solid lubricant. This material has improved wear properties under certain conditions. Material is conductive to electricity and should .. |
|||
Tensile Strength, Yield | 48.3 MPa @Thickness 1.57 mm |
7000 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP347 Cotton Fabric Description: Bleached canvas with high temperature phenolic resin with molybdenum disulfide lubricant. Low moisture absorption. Capable of 150°C continuous operation.Thickness Tested: 0.062", 0.1.. |