Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 461 MPa @Temperature 25.0 °C, Time 11500 sec |
66900 psi @Temperature 77.0 °F, Time 3.20 hour |
As Welded and Solution Annealed at 2075°F(1135°C)/30min/AC; Base/Base Fracture; 0.2% Offset |
Haynes 282® Nickel Alloy Autogenously Welded Sheet Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Tensile Strength, Yield | 461 MPa @Temperature 24.0 °C |
66900 psi @Temperature 75.2 °F |
|
Hexcel® HexPly® F263 Epoxy Resin, 7781 Glass Fabric Hexcel designation: 7781-38"-F263; Fiber: 75-1/0Information provided by HexCel |