Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 451 MPa @Strain 0.200 %, Thickness 3.20 mm |
65400 psi @Strain 0.200 %, Thickness 0.126 in |
as welded |
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Sheet Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |