Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 396 MPa @Temperature 20.0 °C |
>= 57400 psi @Temperature 68.0 °F |
|
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T6 Heat Treatment Condition T6 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Tensile Strength, Yield | 396 MPa @Thickness 12.7 mm, Temperature 316 °C |
57400 psi @Thickness 0.500 in, Temperature 601 °F |
0.2% Offset |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Tensile Strength, Yield | 396 MPa @Strain 0.200 %, Temperature 900 °C |
57400 psi @Strain 0.200 %, Temperature 1650 °F |
|
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Age-hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Tensile Strength, Yield | 396 MPa @Treatment Temp. 427 °C, Time 1.44e+7 sec |
57400 psi @Treatment Temp. 801 °F, Time 4000 hour |
0.2%. Room temp test after thermal exposure |
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |