Polymer Property : Tensile Strength, Yield = 56600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 390 MPa

@Strain 0.200 %
56600 psi

@Strain 0.200 %
Outokumpu Typical,Cold Rolled Strip/Sheet; EN 10002-1
Outokumpu 4372 Cr-Ni Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, and rod forms.
Tensile Strength, Yield 390 MPa

@Strain 1.00 %
56600 psi

@Strain 1.00 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4429 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), cold rolled strip/sheet and rod forms.
Tensile Strength, Yield >= 390 MPa

@Strain 0.200 %,
Thickness 160 - 180 mm
>= 56600 psi

@Strain 0.200 %,
Thickness 6.30 - 7.09 in
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..
Tensile Strength, Yield >= 390 MPa

@Strain 0.200 %
>= 56600 psi

@Strain 0.200 %
Minimum
Aleris Hokotol Aluminum Alloy, 325 mm Thickness
Sample treatment not specified for property data.Applications include molds for blow forming and injection molding for plastics; bolsters and force plates; high strength/low weight machine parts; an..
Tensile Strength, Yield 390 MPa

@Strain 0.200 %,
Thickness 12.7 mm
56600 psi

@Strain 0.200 %,
Thickness 0.500 in
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 1000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications ..