Polymer Property : Tensile Strength, Yield = 54960 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 378.9 MPa

@Strain 0.200 %
54960 psi

@Strain 0.200 %
after porcelain firing
Wieland Simidur Superior PFM Alloy
Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partialsDental