Polymer Property : Tensile Strength, Yield = 51500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 355 MPa

@Strain 1.00 %,
Temperature -80.0 °C
51500 psi

@Strain 1.00 %,
Temperature -112 °F
EN min.; EN 10002-5
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 355 MPa

@Strain 1.00 %,
Temperature -80.0 °C
51500 psi

@Strain 1.00 %,
Temperature -112 °F
EN min.; EN 10002-5
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 355 MPa

@Strain 1.00 %,
Temperature -80.0 °C
51500 psi

@Strain 1.00 %,
Temperature -112 °F
EN min.; EN 10002-5
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 355 MPa

@Strain 1.00 %,
Temperature -80.0 °C
51500 psi

@Strain 1.00 %,
Temperature -112 °F
EN min.; EN 10002-5
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield 355 MPa

@Strain 1.00 %,
Temperature -80.0 °C
51500 psi

@Strain 1.00 %,
Temperature -112 °F
EN min.; EN 10002-5
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 355 MPa

@Strain 1.00 %,
Temperature -80.0 °C
51500 psi

@Strain 1.00 %,
Temperature -112 °F
EN min.; EN 10002-5
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel
Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,..
Tensile Strength, Yield 355 MPa

@Strain 0.200 %
51500 psi

@Strain 0.200 %
Typical
Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel
Description: CLC 17-13-3LN is a nitrogen alloyed austenitic stainless steel with Mo additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior water ..
Tensile Strength, Yield 355 MPa

@Thickness 12.7 mm,
Temperature 427 °C
51500 psi

@Thickness 0.500 in,
Temperature 801 °F
0.2% Offset
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Tensile Strength, Yield >= 355 MPa

@Thickness 16.0 mm
>= 51500 psi

@Thickness 0.630 in
ThyssenKrupp COR-TEN B Structural Steel
This Material Specification applies to plates up to 50 mm in thickness made from COR-TEN B.Definition: Weathering means that due to its chemical composition the COR-TEN B steel, when utilized unprot..
Tensile Strength, Yield 355 MPa

@Strain 0.200 %,
Thickness 15.0 - 35.0 mm
51500 psi

@Strain 0.200 %,
Thickness 0.591 - 1.38 in
Typical Strength
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing ..
Tensile Strength, Yield 355 MPa

@Strain 0.200 %,
Thickness 80.0 - 120 mm
51500 psi

@Strain 0.200 %,
Thickness 3.15 - 4.72 in
Typical Strength
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing ..