Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 303 - 359 MPa @Strain 0.200 % |
43900 - 52100 psi @Strain 0.200 % |
Typical |
AK Steel 18 Cr-Cb™ Ferritic Stainless steel AK Steel 18 Cr-Cb™ provides a more effective solution than Type 409 to many automotive exhaust applications, due to its higher oxidation resistance, improved creep resistance and moderate formabili.. |
|||
Tensile Strength, Yield | 303 - 372 MPa @Strain 0.200 %, Thickness 0.508 - 1.52 mm |
43900 - 54000 psi @Strain 0.200 %, Thickness 0.0200 - 0.0600 in |
|
ATI Allegheny Ludlum 430 Ferritic Stainless Steel Characteristics:oxidation resistant at elevated temperatures, corrosion resistance approaching nickel-bearing stainless steels in mildly corrosive environments, ductile, does not work harden readily.. |
|||
Tensile Strength, Yield | 303 MPa @Thickness 3.20 mm, Temperature 316 °C |
43900 psi @Thickness 0.126 in, Temperature 601 °F |
0.2% offset |
Haynes Hastelloy® C-4 alloy, sheet, heat treated at 1066°C, rapid quenched Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |
|||
Tensile Strength, Yield | 303 MPa @Thickness 3.20 mm, Temperature 427 °C |
43900 psi @Thickness 0.126 in, Temperature 801 °F |
0.2% offset |
Haynes Hastelloy® C-4 alloy, sheet, heat treated at 1066°C, rapid quenched Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |
|||
Tensile Strength, Yield | 303 MPa @Strain 0.200 %, Time 3.60e+6 sec |
43900 psi @Strain 0.200 %, Time 1000 hour |
Room Temperature properties after Isothermal Exposure |
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar.. |
|||
Tensile Strength, Yield | 303 MPa @Strain 0.200 %, Treatment Temp. 760 °C |
43900 psi @Strain 0.200 %, Treatment Temp. 1400 °F |
Room Temperature properties after Isothermal Exposure |
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar.. |