Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 26.0 MPa @Temperature 23.0 °C |
3770 psi @Temperature 73.4 °F |
50 mm/min; ISO 527-2 |
Solvay Specialty Polymers Polidan® TUX 100 Polyethylene, Crosslinked (XLPE) Polidan® TUX 100 is a high density crosslinkable polyethylene compound manufactured according to the Sioplas® process. It has been developed for the production of crosslinked pipes in a wide r.. |
|||
Tensile Strength, Yield | 26.0 MPa @Strain 300 % |
3770 psi @Strain 300 % |
ASTM D-412 |
BASF Elastollan® C-95A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen.. |
|||
Tensile Strength, Yield | 26.0 MPa @Strain 300 % |
3770 psi @Strain 300 % |
ASTM D-412 |
BASF Elastollan® S95A Polyester Type Polyurethane Elastomer Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solv.. |
|||
Tensile Strength, Yield | 26.0 MPa @Strain 100 % |
3770 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® C-64D Polyester Type Polyurethane Elastomer Recommended for injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellent oil, fue.. |