Tensile Strength, Yield 24.0 MPa

@Strain 300 %
3480 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 1055DE Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are Poly(adipate)ester based thermoplastic polyurethanes with good balanced qualities. They exhibit good toughness, abrasive resistance, solvent resistance, and transp..
Tensile Strength, Yield 24.0 MPa

@Strain 300 %
3480 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 1095AF Poly(adipate)ester TPU Resin
ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be inject..
Tensile Strength, Yield 24.0 MPa

@Strain 300 %
3480 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 3095A Polyether TPU Resin
ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod..
Tensile Strength, Yield 24.0 MPa

@Strain 300 %
3480 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 1095A Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products ..
Tensile Strength, Yield 24.0 MPa

@Temperature 121 °C
3480 psi

@Temperature 250 °F
ASTM D638
BASF Ultramid® 8270 HS BK 102 PA6 (Dry)
Description: Ultramid 8270 HS BK-102 is a thermally modified pigmented black, PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile ex..
Tensile Strength, Yield 24.0 MPa

@Strain 100 %
3480 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® C-60D Polyester Type Polyurethane Elastomer
Recommended for injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellent oil, fue..
Tensile Strength, Yield 24.0 MPa

@Strain 100 %
3480 psi

@Strain 100 %
ISO 527-1/-2
DSM Arnitel® UM551 55 Shore D Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 24.0 MPa

@Strain 100 %
3480 psi

@Strain 100 %
ISO 527-1/-2
DSM Arnitel® UM551 Polyether Ester Elastomer (European Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..