Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 221 MPa @Thickness 1.57 mm |
32000 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP510A Glass Fabric Description: Woven glass fabric epoxy laminate. Engineered to provide NEMA grade FR-4 properties. This material contains bromine on the epoxy resin backbone. Certifiable to MIL-I-24768/27, Type GEE-.. |
|||
Tensile Strength, Yield | 220.6 MPa @Temperature 204 °C |
32000 psi @Temperature 399 °F |
|
ATI Allegheny Ludlum AL 468™ Dual Stabilized- Low Titanium Stainless Steel Characteristics:good corrosion resistance in a wide range of environments, can be used in annealed cold formed or as-welded conditions. Applications: used in place of Type 304 in an oxidizing when .. |