Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 22.0 MPa @Strain 0.200 %, Temperature 816 °C |
3190 psi @Strain 0.200 %, Temperature 1500 °F |
|
AK Steel 409 ULTRA FORM® Stainless Steel AK Steel 409 ULTRA FORM Stainless Steel provides an outstanding combination of improved forming and welding characteristics, while providing superior resistance to oxidation, corrosion, ridging and .. |
|||
Tensile Strength, Yield | 22.0 MPa @Strain 100 % |
3190 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® S60D Polyester Type Polyurethane Elastomer Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solv.. |
|||
Tensile Strength, Yield | 22.0 MPa @Strain 100 % |
3190 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® 1160D Polyether Type Polyurethane Elastomer Recommended for injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exh.. |
|||
Tensile Strength, Yield | 22.0 MPa @Strain 300 % |
3190 psi @Strain 300 % |
ASTM D-412 |
BASF Elastollan® C-90A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen.. |