Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 217 MPa @Thickness 9.50 mm, Temperature 649 °C |
31500 psi @Thickness 0.374 in, Temperature 1200 °F |
0.2% offset |
Haynes Hastelloy® C-4 alloy, plate, heat treated at 1066°C, rapid quenched Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang.. |
|||
Tensile Strength, Yield | 217 MPa @Strain 0.200 %, Temperature 371 °C |
31500 psi @Strain 0.200 %, Temperature 700 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Tensile Strength, Yield | 217 MPa @Temperature 204 °C |
31500 psi @Temperature 399 °F |
ASTM E8 |
ATI Allegheny Ludlum 310 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Tensile Strength, Yield | 217 MPa @Strain 0.200 %, Temperature 371 °C |
31500 psi @Strain 0.200 %, Temperature 700 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |