Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 214 MPa @Temperature -40.0 °C |
31000 psi @Temperature -40.0 °F |
ISO 527 |
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Dry) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Tensile Strength, Yield | 214 MPa @Strain 0.200 % |
31000 psi @Strain 0.200 % |
Extruded Bar - Longitudinal |
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy High strength wrought Mg alloy available as rolled plate, forging feedstock, and extrusions. It is a wrought evolution of the casting alloy Elektron WE43. Elektron 43 uses zirconium grain refining.. |
|||
Tensile Strength, Yield | 214 MPa @Strain 0.200 %, Temperature 538 °C |
31000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C) Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |