Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 210 MPa @Strain 0.200 %, Temperature 200 °C |
30500 psi @Strain 0.200 %, Temperature 392 °F |
EN min.; EN 10002-5 |
Outokumpu 4016 Ferritic Stainless Steel Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well su.. |
|||
Tensile Strength, Yield | 210 MPa @Strain 0.200 % |
30500 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Yield | 210 MPa @Strain 0.200 %, Temperature 100 °C |
30500 psi @Strain 0.200 %, Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 4310 Cr-Ni Austenitic Stainless Steel Cold work hardening steel suitable for manufacture of springs operating in corrosive conditions.Available hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and ro.. |
|||
Tensile Strength, Yield | 210 MPa @Strain 0.200 %, Temperature 400 °C |
30500 psi @Strain 0.200 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 4565 High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Tensile Strength, Yield | >= 210 MPa @Strain 0.200 % |
>= 30500 psi @Strain 0.200 % |
|
Industeel CLC 18.15.4L 3% Mo Minimum Austenitic Stainless Steel Description: CLC 18-15-4L (317L) is an austenitic stainless steel with a 3% minimum Molybdenum addition. Alloys CLC 18-15-4L (317L) exhibit austenitic microstructure free of deleterious carbide prec.. |
|||
Tensile Strength, Yield | >= 210 MPa @Strain 0.200 % |
>= 30500 psi @Strain 0.200 % |
|
Industeel NUCL 18.10 B4 Natural Boron (Min 1% wt) Alloyed 304 Stainless Steel Description: Isotope B10 has the property to capture neutrons produced by nuclear reactions. Natural boron contains about 19.9 at% or 18.45 wt % of B10 isotope, the remaining being B11 isotope. NUCL.. |
|||
Tensile Strength, Yield | 210.3 MPa @Thickness 25.4 mm, Temperature 427 °C |
30500 psi @Thickness 1.00 in, Temperature 801 °F |
0.2% offset |
Haynes Hastelloy® C-276 alloy, solution heat treated flat products Hastelloy® C-276 alloy is a nickel-molybdenum-chromium wrought alloy that is a versatile corrosion-resistant alloy. C-276 alloy is an improved wrought version of alloy C in that it usually doesn'.. |