Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 205 MPa @Temperature 20.0 °C |
>= 29700 psi @Temperature 68.0 °F |
|
PEAK Werkstoff DISPAL S250 Aluminum Alloy, AlSi20Fe5Ni2, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Tensile Strength, Yield | 204.8 MPa @Thickness 2.40 mm, Temperature 427 °C |
29700 psi @Thickness 0.0945 in, Temperature 801 °F |
0.2% offset |
Haynes Hastelloy® C-276 alloy, solution heat treated flat products Hastelloy® C-276 alloy is a nickel-molybdenum-chromium wrought alloy that is a versatile corrosion-resistant alloy. C-276 alloy is an improved wrought version of alloy C in that it usually doesn'.. |
|||
Tensile Strength, Yield | 205 MPa @Thickness 9.50 mm, Temperature 760 °C |
29700 psi @Thickness 0.374 in, Temperature 1400 °F |
0.2% offset |
Haynes Hastelloy® C-4 alloy, sheet, aged 100 hours at 899°C Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |
|||
Tensile Strength, Yield | 205 MPa @Strain 0.200 %, Temperature 100 °C |
29700 psi @Strain 0.200 %, Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 904L High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Tensile Strength, Yield | 205 MPa @Strain 1.00 %, Temperature 200 °C |
29700 psi @Strain 1.00 %, Temperature 392 °F |
EN min.; EN 10002-5 |
Outokumpu 904L High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |