Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 14.0 MPa @Strain 50.0 % |
2030 psi @Strain 50.0 % |
ISO 527-1/-2 |
DSM Arnitel® PL471 45 Shore D, Injection Grade Copolyester Elastomer (North America)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 14.0 MPa @Strain 5.00 % |
2030 psi @Strain 5.00 % |
ISO 527-1/-2 |
DSM Arnitel® UM622 General Purpose Grade Copolyester Elastomer (North America)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 14.0 MPa @Strain 5.00 % |
2030 psi @Strain 5.00 % |
ISO 527-1/-2 |
DSM Arnitel® UM622 Polyether Ester Elastomer (European Grade)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 14.0 MPa @Strain 300 % |
2030 psi @Strain 300 % |
ASTM D-412 |
BASF Elastollan® S85A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fue.. |
|||
Tensile Strength, Yield | 14.0 MPa @Strain 100 % |
2030 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® S95A Polyester Type Polyurethane Elastomer Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solv.. |
|||
Tensile Strength, Yield | 14.0 MPa @Strain 50.0 % |
2030 psi @Strain 50.0 % |
ISO 527-1/-2 |
DSM Arnitel® PL471 Polyether Ester Elastomer (European Grade)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |