Mechanical Properties Metric English Comments
Tensile Strength, Yield 132 MPa

@Strain 0.200 %,
Temperature 300 °C
19100 psi

@Strain 0.200 %,
Temperature 572 °F
EN min.; EN 10002-5
Outokumpu 4878 High Temperature Austenitic Stainless Steel
Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For ..
Tensile Strength, Yield 132 MPa

@Temperature 982 °C,
Time 11500 sec
19100 psi

@Temperature 1800 °F,
Time 3.20 hour
As Welded, Solution Annealed, and Aged; Base/Weld Fracture; 0.2% Offset
Haynes 282® Nickel Alloy Autogenously Welded Sheet
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..