Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1280 MPa @Temperature 20.0 °C |
185000 psi @Temperature 68.0 °F |
45 HRC |
EDRO #5 H13-Hot Work Tool Steel EDRO #5™ H13 is a chromium-molybdenum-vanadium-alloyed steel characterized by: good resistance to thermal shock and thermal fatigue, good high-temperature strength, good toughness and ductility, go.. |
|||
Tensile Strength, Yield | 1280 MPa @Strain 0.200 % |
185000 psi @Strain 0.200 % |
H900 |
Crucible Steel 15-5 Precipitation Hardening Stainless Steel Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V.. |
|||
Tensile Strength, Yield | 1280 MPa @Strain 0.200 % |
185000 psi @Strain 0.200 % |
H900 |
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a.. |
|||
Tensile Strength, Yield | 1280 MPa @Strain 0.200 % |
185000 psi @Strain 0.200 % |
H900 |
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. .. |
|||
Tensile Strength, Yield | 1280 MPa @Strain 0.200 % |
185000 psi @Strain 0.200 % |
hardened to 45 HRC |
Bohler-Uddeholm ORVAR® 2M / AISI H13 Hot Work Tool Steel Orvar 2 Microdized is a chromium-molybdenum-vanadium alloyed steelORVAR® 2M / AISI H13 is a conventionally produced hot work tool steel with overall good ductility, toughness, wear resistance, hard.. |
|||
Tensile Strength, Yield | 1280 MPa @Strain 0.200 % |
185000 psi @Strain 0.200 % |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM ORVAR® SUPERIOR (Premium AISI H13) Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o.. |
|||
Tensile Strength, Yield | 1280 MPa @Strain 0.200 % |
185000 psi @Strain 0.200 % |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o.. |
|||
Tensile Strength, Yield | 1280 MPa @Strain 0.200 % |
185000 psi @Strain 0.200 % |
hardened to 45 HRC |
Bohler-Uddeholm UDDEHOLM STAVAX® ESR Modified 420 Premium grade stainless tool steelStavax® ESR is characterized by: Good corrosion resistance Good polishability Good wear resistance Good machinability Good stability in hardeningApplications: Udd.. |