Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 12.3 MPa @Strain 10.0 % |
1780 psi @Strain 10.0 % |
ASTM D638 |
SK Chemicals SKYPEL G155D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Tensile Strength, Yield | 12.3 MPa @Strain 100 % |
1780 psi @Strain 100 % |
ASTM D412 |
SK Chemicals SKYTHANE® 195A R series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Yield | 12.3 MPa @Strain 10.0 % |
1780 psi @Strain 10.0 % |
ASTM D638 |
SK Chemicals SKYPEL P155D Productivity Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |