Polymer Property : Tensile Strength, Yield = 161300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1112 MPa

@Strain 0.200 %
161300 psi

@Strain 0.200 %
Transverse
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 1075
AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, ..