Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 82.0 MPa @Strain 0.200 %, Temperature 600 °C |
11900 psi @Strain 0.200 %, Temperature 1110 °F |
EN min.; EN 10002-5 |
Outokumpu 4828 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Tensile Strength, Yield | 82.0 MPa @Strain 0.200 %, Temperature 600 °C |
11900 psi @Strain 0.200 %, Temperature 1110 °F |
EN min.; EN 10002-5 |
Outokumpu 4833 High Temperature Austenitic Stainless Steel Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and .. |
|||
Tensile Strength, Yield | 82.0 MPa @Strain 0.200 %, Temperature 600 °C |
11900 psi @Strain 0.200 %, Temperature 1110 °F |
EN min.; EN 10002-5 |
Outokumpu 4845 High Temperature Austenitic Stainless Steel Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o.. |
|||
Tensile Strength, Yield | 82.0 MPa @Temperature 23.0 °C |
11900 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 82.0 MPa @Temperature 23.0 °C |
11900 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 101L BKB080 Nylon 66
(Unverified Data**) Zytel® 101L BKB080 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 82.0 MPa @Temperature 649 °C |
11900 psi @Temperature 1200 °F |
|
ATI Allegheny Ludlum AL 453™ Stainless Steel Single phase iron-chromium ferritic stainless steel alloy. Should be annealed between 1450 and 1600°F and quickly cooled. Information provided by Allegheny Ludlum |
|||
Tensile Strength, Yield | 82.0 MPa @Temperature 371 °C |
11900 psi @Temperature 700 °F |
|
ATI Wah Chang Zircadyne® Alloy Zr 702 Zircadyne 702 is commercially pure zirconium. Alloy exhibits good ductility even at cryogenic temperatures and good strength comparable with other common engineering alloys.Information provided by A.. |
|||
Tensile Strength, Yield | 82.0 MPa @Temperature 23.0 °C |
11900 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® FG101L NC010 Nylon 66
(Unverified Data**) Zytel® FG101L NC010 is a lubricated polyamide 66 resin for injection molding. It has been developed for consideration into applications such as parts for the food industry.Information provided by D.. |