Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 699 MPa @Strain 0.200 %, Temperature 25.0 °C |
101000 psi @Strain 0.200 %, Temperature 77.0 °F |
|
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Age-hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Tensile Strength, Yield | 696 MPa @Strain 0.200 %, Diameter 12.7 mm |
101000 psi @Strain 0.200 %, Diameter 0.500 in |
As Welded, Solution Annealed, and Aged |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |