Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 758 - 889 MPa @Strain 0.200 %, Thickness >=25.4 mm |
110000 - 129000 psi @Strain 0.200 %, Thickness >=1.00 in |
Cold Drawn Bars |
Schmolz + Bickenbach 416RS Stainless Steel Bar Description: Ugitech’s 416RS is a low sulfur pre-hardened chrome bearing martensitic stainless steel specifically designed for the precision rifle barrel industry. The 416RS chemistry is balanc.. |